Title: Development of Standard Plans for Glulam Highway Bridges

Source: FPL RIP-4719-011

Author(s)Wacker, James

Publication Year: 2010  View PDF »

Related Publications: view

Category: Research In Progress

Abstract: The main emphasis of this project will be updating available glued-laminated timber (glulam) bridge design standards to meet the 2007 AASHTO-LRFD Bridge Design Specifications. There is a need to provide basic engineering guidance to practicing engineers regarding the design and fabrication of timber bridge systems. Engineering design aids in the form of standard plan drawings, details, and specifications have proven to be effective guidance tools.

Keywords: glulam, bridges, design standards; timber bridges, bridge design

File size: 406 kb(s)

Date posted: 09/13/2010
Current FPL Scientist associated with this product
Wacker, James P.
Research General Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »