Title: Development of a Do-It-Yourself Tornado Safe Room from Commodity Wood Products

Source: USDA Forest Service, Forest Products Laboratory, Madison, Wisconsin, Research In Progress FPL-RIP-4714-028

Author(s): Forest Products Laboratory

Publication Year: 2014  View PDF »

Related Publications: view

Category: Research In Progress

Abstract: Every year in the United States, tornados result in more than 80 deaths and 1,500 injuries. These numbers could be reduced if tornado safe rooms were more common. Although many safe room designs exist and function adequately, they are either very expensive or require professionals to construct. The development of an economical safe room constructed of commonly available wood building materials and buildable by a do-it-yourselfer would help make the availability and use of these structures more widespread.

Keywords: tornado, safe room, lumber, do-it-yourself

File size: 805 kb(s)

Date posted: 06/15/2014

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »