Title: Biohybrid hydrogel and aerogel from self-assembled nanocellulose and nanochitin as a high-efficiency adsorbent for water purification

Source: Res. in Prog. RIP-4707-003. Madison, Wisconsin: U.S. Department of Agriculture, Forest Service, Forest Products Laboratory. 2 p.

Author(s)Hassan, El Barbary; Schueneman, Greg

Publication Year: 2020  View PDF »

Related Publications: view

Category: Research In Progress

Abstract: Water purification for drinking or safe discharge into the environment after usage is a growing problem worldwide. Industrialized countries have regulations, systems, and means, while developing countries have much fewer resources. This research investigates inexpensive and effective water filtration media that can be readily made from wood including waste or scrap sources in combination with chitin that can be extracted from algae or more plentiful sources such as waste crab or shrimp shells.

Keywords: water purification; pollution; biobased; filtration; nanocellulose

Publication Review Process: Non-Refereed (Other)

File size: 416 kb(s)

Date posted: 10/02/2020
RITS Product ID: 10028
Current FPL Scientist associated with this product
Schueneman, Gregory
Supervisory Research Materials Engineer
  

Additional items that might interest you
View the video celebrating FPL's 100 years of public service in 2010, from the producers of the Greatest Good....view

Research Highlights from FPL....view

Termite Eradication: A search for the Holy Grail.... view

Moisture Management in Residential Construction Series videos...view

Wood Floor Systems in Residential Construction Series videos....view
- FPL's Mission and Strategic Plan -

FPL's mission is to identify and conduct innovative wood and fiber utilization research that contributes to conservation and productivity of the forest resource, thereby sustaining forests, the economy, and quality of life. ... ..more »

- FPL Research Emphasis Areas -
Advanced Composites

As an integral part of the FPL mission, we improve the long-term sustainability of our Nation's forests by creating valuable composite products from biobased materials ... ..more »


Advanced Structures

The FPL has been in the forefront of wood-frame housing research since 1910 and has long been recognized as a world leader in such housing-related areas as engineered wood ... ..more »


Forest Biorefinery

We all know the compelling reasons that the United States needs to reduce its dependence on fossil fuels. Historically, the greatest increases in energy demand have been for transportation fuels ... ..more »


Nanotechnology

A leader in wood products research for over a century, the FPL is positioning itself to become the lead Federal research facility for the application of nanotechnology in forest products ... more »


Woody Biomass Utilization

Forests in the United States contain a substantial amount of small-diameter, overstocked, and underutilized material.FPL research projects are exploring the potential of the small-diameter ... ..more »